Stainless steel wire AISI 302 hard according to EN 10270/3

TECHNICAL SHEET

Quality: Austenitic steel with good mechanical properties and corrosion resistance

Finishing:
– bright (max Ø mm 4.00)
– stearate coated (Ø mm 0.20 – 12.00)

Diameters: from mm 0.10 to mm 12.00
Tolerances according to EN 10270/3

Chemical composition according to EN10270/2:

% C % Mn max % Si max % P max % S max % Mo % Cr % Ni
0.05 – 0.15 2.00 2.00 0.045 0.015  ≤ 0.80 16 – 19 6.00 – 9.50

Packaging: coil, spools and bars.

Operating temperatures: -200 + 250°C max

Heat treatment after coiling of finished parts:

TEMPERATURE: 350°/425°
TIME: 1 – 3 h
INCREASE OF TENSILE N/mm²: 60-200

Mechanical properties:
Elasticity E: longitudinal state of supply N/mm² 180.000, after heat treatment N/mm² 185.000
Elasticity G: transverse state of supply N/mm² 70.000, after heat treatment N/mm² 73.000

Stainless steel wire resistance table 10270/3

fili-acciaio-inossidabile_01

APPLICATIONS

  • Springs.
  • Engineered components.
  • Wire mesh.
  • Wire cloth.
  • Hose braiding.

REFERENCE STANDARDS

  • EN 10270/3
  • X10CrNi18-8 Nr 1.4310
  • DIN 17224/82
  • AISI 302

Do you need more information or quotation?