Quality: Austenitic stianless wire with Molibden, this element provides better corrosion resistance and non-magnetic properties than 302 & 304 stainless, in marine and industrial applications.
Better pitting and crevice corrosion resistance than 302 & 304 stainless.
Finishing:
– bright
– stearate
Diameter: from mm 0.30 to mm 4.00 (bright)
from mm 0.30 to mm 10.00 (stearate)
Tolerances according to EN 10270/3
Chemical composition according to EN 10270-3 (1.4401):
% C | % Mn max | % Si max | % P max | % S max | % Mo | % Cr | % Ni |
≤ 0.07 | 2.00 | 1.00 | 0.045 | 0.015 | 2.00 – 2.50 | 16.50 – 18.50 | 10 – 13 |
Chemical composition according to 1.4404:
% C | % Mn max | % Si max | % P max | % S max | % Mo | % Cr | % Ni |
≤ 0.03 | 2.00 | 1.00 | 0.045 | 0.015 | 2.00 – 2.50 | 16.50 – 18.50 | 10 – 13 |
Packaging: coil, spools and bars.
Operating temperature: -200 + 250°C max
Heat treatment after coiling of finished parts:
TEMPERATURE: 350°/425°
TIME: 30min – 4 h
INCREASE OF TENSILE N/mm²: 60-150
Mechanical properties
Elasticity E: longitudinal state of supply N/mm² 175.000, after heat treatment N/mm² 180.000
Elasticity G: transverse state of supply N/mm² 68.000, after heat treatment N/mm² 71.000
Tabella resistenza filo inox EN 10270/3